Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 53Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum Melted, Solution Heat Treated Precipitation Hardenable
€68.00
Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 48Ni - 20Cr - 20Co - 5.9Mo - 2.2Ti - 0.45Al Consumable Electrode or Vacuum Induction Melted Solution Heat Treated
€73.00
Steel, Corrosion-Resistant, Sheet and Strip 18Cr - 9.0Ni (SAE 30302) Cold Rolled, Full Hard, 185 ksi (1276 MPa) Tensile Strength
€70.00
Steel, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 17Cr - 12Ni - 2.5Mo (SAE 30316) Cold Rolled, 1/4 Hard, 125 ksi (862 MPa) Tensile Strength
Steel, Corrosion-Resistant, Sheet, Strip, and Plate 19Cr - 9.2Ni (SAE 30304) Cold Rolled, 125 ksi (862 MPa) Tensile Strength
Steel, Corrosion-Resistant, Sheet, Strip, and Plate 18Cr - 9.0Ni (SAE 30302) Cold Rolled, 1/4 Hard, 125 ksi (862 MPa) Tensile Strength
Steel, Corrosion-Resistant, Sheet and Strip 18Cr - 9.0Ni (SAE 30302) Cold Rolled, 1/2 Hard, 150 ksi (1034 MPa) Tensile Strength
Steel, Corrosion-Resistant, Sheet and Strip 18Cr - 9.0Ni (SAE 30302) Cold Rolled, 3/4 Hard, 175 ksi (1207 MPa) Tensile Strength
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti Consumable Electrode Remelted or Vacuum Induction Melted 1750 °F (954 °C) Solution Heat Treated
Aluminum Alloy Extrusions 4.4Cu - 1.5Mg - 0.60Mn (2024-T3) Solution Heat Treated
Aluminum Alloy, Plate 6.2Zn - 1.9Cu - 2.1Mg - 0.10Zr (7040-T7451) Solution Heat Treated, Stress Relieved, and Overaged
Aluminum Alloy, Plate (7140-T7651) 6.6Zn - 1.8Cu - 2.0Mg - 0.10Zr Solution Heat Treated, Stress Relieved, and Overaged
Nickel Alloy, Corrosion and Heat-Resistant, Investment Castings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb(Nb) - 0.90Ti - 0.60Al - 18Fe Vacuum Melted Homogenization and Solution Heat Treated
Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, Foil and Plate 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated
Steel, Corrosion-Resistant, Wire 18Cr - 9.0Ni (SAE 30302) Spring Temper