DIN EN 60317-60:2013-04

Specifications for particular types of winding wires - Part 60: Polyester glass fibre wound minimum class 155 resin or varnish impregnated or not impregnated, bare or enamelled, rectangular copper wire, temperature index 155 (IEC 60317-60:2012); German version EN 60317-60:2012.

Summary

This part of IEC 60317 specifies requirements of polyester glass fibres wound impregnated or not impregnated, bare, or grade 2 enamelled rectangular copper winding wire, temperature index 155. If used, the impregnating agent can be, for instance, polyester or polyesterimide resin based.

Notes

A transition period, as set out in DIN EN IEC 60317-60-1 (2021-11) and DIN EN IEC 60317-60-2 (2021-11), exists until 2023-07-27.*Applies in conjunction with DIN EN 60317-0-8 (2013-06)