Fine ceramics (advanced ceramics, advanced technical ceramics) — Test method for GaN crystal surface defects — Part 2: Method for determining etch pit density
Summary
This document describes a method for determining the etch pit density, which is used to detect dislocations and processing-introduced defects that occur on single-crystal GaN substrates or single-crystal GaN films.
It is applicable to the defects specified in ISO 5618-1 from among the defects exposed on the surface of the following types of GaN substrates or films: single-crystal GaN substrate; single-crystal GaN film formed by homoepitaxial growth on a single-crystal GaN substrate; or single-crystal GaN film formed by heteroepitaxial growth on a single-crystal Al2O3, SiC, or Si substrate.
It is applicable to defects with an etch pit density of = 7 × 107 cm-2.
Technical characteristics
| Publisher | Bureau de Normalisation Belge (NBN) |
| Publication Date | 10/10/2024 |
| Page Count | 0 |
| EAN | --- |
| ISBN | --- |
| Weight (in grams) | --- |
No products.